Simple to use

1 step: deposit + fusing
Strong bonding
0,2-12 mm thickness 
Smoother surface

Basically this method uses a simple oxy-acetylene torch. Finely divided powder (100 - 10 micron) is fed through an injector from the hopper into the flame.

Powder welding is used for deposits between 0,2 mm and 12 mm, both for repairs and original parts. This method is especially suitable for building up edges and corners.

Deposition rate 0,5-2,5 kg/hour

Deposition thickness 0,2 - 12 mm

Deposition hardness  20 - 62 HRC